Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking

Product Details
Customization: Available
CAS No.: 1305-78-8
Formula: Cao
Diamond Member Since 2018

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

High Repeat Buyers Choice
More than 50% of buyers repeatedly choose the supplier
Years of Export Experience
The export experience of the supplier is more than 10 years
Patents Awarded
The supplier had awarded 1 patents, you can check the Audit Report for more information
Exhibition Experience
The supplier had participated in offline trade shows, you can check the Audit Report for more information
to see all verified strength labels (17)
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
  • Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
Find Similar Products

Basic Info.

Model NO.
SCA-I, SCA-II
EINECS
215-137-3
Certification
MSDS
Application
Concrete Demolition
Type
SCA-I
Condition
100% New
Delivery
20-30days
MOQ
1tons
Color
Gray
After Sale Service
Yes
Transport Package
Carton, Pallet
Specification
5kgs per bag, 20kgs per carton
Trademark
SANSUNG
Origin
China
HS Code
3824999909
Production Capacity
20000tons/Year

Product Description

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking


What's CRACK AGENT / Expansive Mortar?

CRACK AGENT (Expansive Mortar) is a kind of powder with amazing 18,000 PSI expansive strength when mixed with common water. Poured into holes, CRACK AGENT breaks reinforced concrete & rock safely and quietly, while providing SILENT cracking. Since CRACK AGENT provides controlled demolition according to drilling patterns, it is very easy to break reinforcedconcrete and all kinds of stone into desired sizes and shapes, without noise, vibration or dust.

In demolition, concrete cutting & excavating industry, CRACK AGENT helps you to break reinforced concrete and rock into chunks, so you may easily cut off rebar, haul it away with a crane or truck without damage remaining part.

 

In mining and quarrying industry, CRACK AGENT helps to achieve perfect slabs and blocks from limestone, onyx, marble, granite or any other type of stone you are working with. Compares to blasting, CRACK AGENT avoids waste of valuable stone, high insurance, costly storage and labor. CRACK AGENT can also be applied along with traditional methods like primer cord, hydraulic breaker, diamond blade saw and jackhammer to help cut cost, work time and increase safety, Plus silent operation, CRACK AGENT is perfect for residential, school and airport area. CRACK AGENT helps your work to become more efficient and cost effective.

Depending on different working temperature, there are four types of crack agent for your choice.

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
 

How to use

Drilling

1. Drill holes using an air hammer drill and appropriate drill bit specific to the rock type.

2. Holes should be drilled no further than 30-60cm (1ft-2ft) apart. Note: In reinforced concrete recommended no more than 20cm (8") apart.

3. Recommended hole diameter 38mm - 50mm (1 ½" - 2.0"). Depth would be 70-90% of the way depending on the type of rock/material to be removed.

Mixing

1. For regular safety reasons and mixing small amounts by hand, it is recommended to use rubber gloves.

2. In a bucket, combine 1.5 Liters of water to one 5kgs bag of CRACK AGENT. Or pour water and CRACK AGENT as a rate of 1:3 units by weight.

3. Mix well, using a drill and paddle is recommended. If mixing with a stick or other method, make sure powder is completely dissolved into the water. Mix to a slurry.

Filling

1. Clean holes before filling using air hose remove excess dust from drilling.

2. CRACK AGENT slurry should be poured into holes within 10-15 min. after mixing. Do not fill to the top, only fill the holes about 15mm ( ½" to 1") from the top.

3. Mix well and pour into holes while agitating the hole to make sure no air gaps are in the hole. Example: Using a piece of rod or stick to poke holes.

4. For Horizontal holes, a grouting pump would be most reliable to poor.

Cracking

The cracks appear in 40-60 min. after filling, depending on the weather,rocks, and concrete type. The cracks become wider within time (maximun 48 hours expanding time).

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking

 

Consumption


Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
 

Benefits

1. Amazing Expansive Capability

Amazing 18,000 PSI expansive strength when mixed with common water.

2. Easy to use

No training required before use. Just mix with water and then fill into holes. Once mixed with clean water, CRACK AGENT can be poured into holes pre-drilled in the material you are working with It can be poured into the same holes that dangerous explosives are usually placed in.

3. Non-Explosive & Environmentally Friendly

An alternative to blasting, diamond blade saw, hydraulic breaker and jackhammer, which is safer, more efficient, works without noise, vibration, dust by providing silent expansive cracking.

4. Works Efficiently and Cost Effectively

No Special License, training or equipment needed.

Package

1. First step: 5kg in plastic bag
2. Second step: 4 plastic bags in 1 carton
3. Third step: 50-60 cartons on every wooden or plastic pallet.

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
 

Tips

  • Well designed hole drilling pattern will minimize consumption of CRACK AGENT by cutting into desired sizes.

  • To insure success, CRACK AGENT needs FREE SPACE to expand to.

  • For better results, it is important to note both air and material temperature. Material temperature is the temperature inside of the rock or concrete which can be different from the air temperature.

  • In summer, the best time to use CRACK AGENT is in the evening when material temperature is cool.

  • In summer, cover holes from direct sunlight to avoid blow-out. Example: using a tarp or damp hay to provide shade.

  • If CRACK AGENT completely dries into powder and did NOT crack, pour additional water onto CRACK AGENT filled holes.

  • When using CRACK AGENT on highly absorbent materials like concrete, the holes should be dampened before the mortar is poured, making sure however, that there is no presence of water.

  • Fresh mortar should be poured into holes within 5 minutes after mixing.

  • The workers need to take synchronized operation, especially to hard stone. The quantity of holes each worker responsible to fill has to be moderate. Taking synchronized steps when mixing, stirring and filling will lead to maximum expansive stress with all holes expand at the same time.

  • When mixing, if CRACK AGENT begins to steam in container, add some water to dilute and process properly.

 

Safety Precautions

•Make sure that everyone working with CRACK AGENT understands the possibility of blowouts, and has read the technical instructions thoroughly.

•CRACK AGENT is a highly alkaline product, pH reaches 13 after contact with water and can cause severe irritation to mucous membranes, especially eyes. Skin and eye contacts with CRACK AGENT must be rinsed off with large amounts of cold water immediately without rubbing. Consult a doctor quickly.

•Wear safety goggles and rubber gloves during CRACK AGENT handling, mixing and filling. Dust-proof mask is recommended in poorly ventilated areas such as tunnels or mines.

•Plug the holes immediately after filling and cover the holes with straw mat. Keep your face away from the holes filled by mortar. Stay away from filled holes at least 3 hours after filling to avoid blow-out shot. Keep people away from job site after filling .

•Warm or bubbling mortar is forbidden to fill into holes. Once filled holes start to smoke or steam, that is the sign they may be about to blow out. Clear the area of people immediately.

•Keep people away from jobsite after filling holes. In case of people have to remain in the area, cover filled holes with a tarpaulin.

•Take care of fall of cracked block from the cracking object.

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking

Controlled Demolition Expansive Mortar for Rock Cracking and Concrete Breaking
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier